Gelest
GEL-MCR-A11-100G
不对称单胺基丙基封端的聚二甲基硅氧烷,8-12 cSt
现货
100g
¥6061
不对称单胺基丙基封端的聚二甲基硅氧烷,8-12 cSt
MONOAMINOPROPYL TERMINATED POLYDIMETHYLSILOXANE, asymmetric, 8-12 cSt
货号:GEL-MCR-A11-100G
/
分子量:800-1,200
/
Gelest
GEL-PP2-OE43-1KG
密封胶
现货
1kg
¥6228
密封胶
GELEST® OE 43
货号:GEL-PP2-OE43-1KG
/
Gelest
GEL-SIA0078.0-25G
95%
2-[(乙酰氧基(聚乙烯基乙氧基)丙基]三乙氧基硅烷,95%
现货
25g
¥2717
2-[(乙酰氧基(聚乙烯基乙氧基)丙基]三乙氧基硅烷,95%
2-[(ACETOXY(POLYETHYLENEOXY)PROPYL]TRIETHOXYSILANE, 95%
货号:GEL-SIA0078.0-25G
/
分子量:500-700
/
纯度:95%
/
Gelest
GEL-SIH6188.0-25G
97%
[羟基(聚乙烯氧)丙基]三乙氧基硅烷,(8-12 EO),50%乙醇溶液
现货
25g
¥3051
[羟基(聚乙烯氧)丙基]三乙氧基硅烷,(8-12 EO),50%乙醇溶液
[HYDROXY(POLYETHYLENEOXY)PROPYL]TRIETHOXYSILANE, (8-12 EO), 50% in ethanol
货号:GEL-SIH6188.0-25G
/
分子量:575-750
/
纯度:97%
/
Gelest
GEL-PP1-HSAP-100G
HARDSIL(TM) AP
7到14天内
100g
¥1045
HARDSIL(TM) AP
HARDSIL™ AP
货号:GEL-PP1-HSAP-100G
/
Gelest
GEL-AKT841-100G
95%
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
7到14天内
100g
¥5392
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
货号:GEL-AKT841-100G
/
分子式:C32H66O14Ti(approx)
/
分子量:660-780
/
纯度:95%
/
Gelest
GEL-AKY921.2-5G
97%
YTTERBIUM 3,5-HEPTANEDIONATE
7到14天内
5g
¥6228
YTTERBIUM 3,5-HEPTANEDIONATE
YTTERBIUM 3,5-HEPTANEDIONATE
货号:GEL-AKY921.2-5G
/
分子式:C21H33O6Yb
/
分子量:554.53
/
纯度:97%
/
Gelest
GEL-DBP-V102-1KG
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 c
7到14天内
1kg
¥15549
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 c
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 cSt
货号:GEL-DBP-V102-1KG
/
分子量:9,000-12,000
/
Gelest
GEL-AKC253.5-10G
97%
COPPER(II) METHACRYLOXYETHYLACETOACETATE
7到14天内
10g
¥2299
COPPER(II) METHACRYLOXYETHYLACETOACETATE
COPPER(II) METHACRYLOXYETHYLACETOACETATE
货号:GEL-AKC253.5-10G
/
分子式:C20H26CuO10
/
分子量:489.96
/
纯度:97%
/
Gelest
GEL-DALTI50-500G
97%
ALUMINUM TITANIUM (0.85 M)
7到14天内
500g
¥4702
ALUMINUM TITANIUM (0.85 M)
ALUMINUM TITANIUM (0.85 M)
货号:GEL-DALTI50-500G
/
分子式:Al2Ti(OR)x
/
纯度:97%
/
Gelest
GEL-DGM-000-100G
DIMETHYLSILOXANE GUM
7到14天内
100g
¥1463
DIMETHYLSILOXANE GUM
DIMETHYLSILOXANE GUM
货号:GEL-DGM-000-100G
/
Gelest
GEL-AKT843-100G
97%
TITANIUM ALLYLACETOACETATETRAIISOPROPOXIDE
7到14天内
100g
¥7106
TITANIUM ALLYLACETOACETATETRAIISOPROPOXIDE
TITANIUM ALLYLACETOACETATETRIISOPROPOXIDE
货号:GEL-AKT843-100G
/
分子式:C16H30O6Ti
/
分子量:358.25
/
纯度:97%
/
Gelest
GEL-DMS-Hm25-1KG
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 500 cSt
7到14天内
1kg
¥19855
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 500 cSt
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 500 cSt
货号:GEL-DMS-Hm25-1KG
/
分子量:17,200
/
Gelest
GEL-SST-3PV1-100G
聚(苯基-乙烯基倍半硅氧烷),90%苯基,10%乙烯基
7到14天内
100g
¥3197
聚(苯基-乙烯基倍半硅氧烷),90%苯基,10%乙烯基
POLY(PHENYL-VINYLSILSESQUIOXANE), 90% PHENYL, 10% VINYL
货号:GEL-SST-3PV1-100G
/
分子量:1,000-1,300
/
Gelest
GEL-DCS-8024-100G
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
7到14天内
100g
¥2717
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
货号:GEL-DCS-8024-100G
/
分子量:5,000-6,000
/
Gelest
GEL-SIT8412.0-25G
97%
N-三甲氧基硅丙基-N,N,N-三正丁基溴化铵,50%甲醇溶液
7到14天内
25g
¥3260
N-三甲氧基硅丙基-N,N,N-三正丁基溴化铵,50%甲醇溶液
N-Trimethoxysilylpropyl-N,N,N-tri-n-butylammonium bromide, 50% in methanol
货号:GEL-SIT8412.0-25G
/
分子式:C18H42BrNO3Si
/
分子量:428.52
/
纯度:97%
/
Gelest
GEL-PP1-ZPUE-100G
耐磨涂层(PP1-ZPUE)
7到14天内
100g
¥3302
耐磨涂层(PP1-ZPUE)
ZIPCONE™ UE
货号:GEL-PP1-ZPUE-100G
/
Gelest
GEL-AKT852-25G
97%
双己酸乙酯化二正丁氧基化钛
7到14天内
25g
¥2487
双己酸乙酯化二正丁氧基化钛
TITANIUM DI-n-BUTOXIDE BIS(2-ETHYLHEXANOATE)
货号:GEL-AKT852-25G
/
分子式:C24H48O6Ti
/
分子量:480.52
/
纯度:97%
/
Gelest
GEL-DMGAL50-25G
97%
MAGNESIUM ALUMINUM (1.0M)
7到14天内
25g
¥836
MAGNESIUM ALUMINUM (1.0M)
MAGNESIUM ALUMINUM (1.0M)
货号:GEL-DMGAL50-25G
/
分子式:MgAl(OR)x
/
纯度:97%
/
Gelest
GEL-UTT-1012-100G
丙烯酸丙酯T-构型硅氧烷
7到14天内
100g
¥4096
丙烯酸丙酯T-构型硅氧烷
ACRYLOXYPROPYL T-STRUCTURE SILOXANE, 10-30 cSt
货号:GEL-UTT-1012-100G
/
分子量:500-900
/
Gelest
GEL-AKT878-25G
97%
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
7到14天内
25g
¥1337
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
货号:GEL-AKT878-25G
/
分子式:C19H34O8Ti
/
分子量:438.38
/
纯度:97%
/
Gelest
GEL-DBP-V102-100G
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 c
7到14天内
100g
¥2612
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 c
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 800-1,000 cSt
货号:GEL-DBP-V102-100G
/
分子量:9,000-12,000
/
Gelest
GEL-DLINB050-25G
97%
LITHIUM NIOBIUM (0.85 M)
7到14天内
25g
¥3950
LITHIUM NIOBIUM (0.85 M)
LITHIUM NIOBIUM (0.85 M)
货号:GEL-DLINB050-25G
/
分子式:LiNb(OR)x
/
纯度:97%
/
Gelest
GEL-ATM-1322M50-100G
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
7到14天内
100g
¥376
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
货号:GEL-ATM-1322M50-100G
/
Gelest
GEL-PP2-RG07-1KG
GELEST®hPDMS:高模量硅橡胶
7到14天内
1kg
¥6897
GELEST®hPDMS:高模量硅橡胶
GELEST® hPDMS: HIGH MODULUS REPROGRAPHIC SILICONE
货号:GEL-PP2-RG07-1KG
/
Gelest
GEL-AKS793-25G
97%
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
7到14天内
25g
¥982
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
货号:GEL-AKS793-25G
/
分子式:C8H18O4Sr
/
分子量:297.84
/
纯度:97%
/
Gelest
GEL-DALTI50-100G
97%
ALUMINUM TITANIUM (0.85 M)
7到14天内
100g
¥1212
ALUMINUM TITANIUM (0.85 M)
ALUMINUM TITANIUM (0.85 M)
货号:GEL-DALTI50-100G
/
分子式:Al2Ti(OR)x
/
纯度:97%
/
Gelest
GEL-DMGTI50-25G
97%
MAGNESIUM TITANIUM (1.0M)
7到14天内
25g
¥836
MAGNESIUM TITANIUM (1.0M)
MAGNESIUM TITANIUM (1.0M)
货号:GEL-DMGTI50-25G
/
分子式:MgTi(OR)x
/
纯度:97%
/
Gelest
GEL-AKS793-100G
97%
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
7到14天内
100g
¥3176
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
STRONTIUM 1-METHOXY-2-PROPOXIDE, 18-20% in methoxypropanol
货号:GEL-AKS793-100G
/
分子式:C8H18O4Sr
/
分子量:297.84
/
纯度:97%
/
Gelest
GEL-DBAZR50-25G
97%
BARIUM ZIRCONIUM (0.33 M)
7到14天内
25g
¥1065
BARIUM ZIRCONIUM (0.33 M)
BARIUM ZIRCONIUM (0.33 M)
货号:GEL-DBAZR50-25G
/
分子式:BaZr(OR)x
/
纯度:97%
/
Gelest
GEL-DMS-CA21-1KG
双(羟乙基)氨基封端的聚二甲基硅氧烷,120-160 cSt
7到14天内
1kg
¥29260
双(羟乙基)氨基封端的聚二甲基硅氧烷,120-160 cSt
[BIS(HYDROXYETHYL)AMINE] TERMINATED POLYDIMETHYLSILOXANE, 120-160 cSt
货号:GEL-DMS-CA21-1KG
/
分子量:3000
/
Gelest
GEL-DBATI50-25G
97%
BARIUM TITANIUM (0.5 M)
7到14天内
25g
¥961
BARIUM TITANIUM (0.5 M)
BARIUM TITANIUM (0.5 M)
货号:GEL-DBATI50-25G
/
分子式:BaTi(OR)x
/
纯度:97%
/
Gelest
GEL-DMA-131-100G
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
7到14天内
100g
¥1588
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
货号:GEL-DMA-131-100G
/
Gelest
GEL-DMS-Hm21-1KG
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
7到14天内
1kg
¥18998
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
货号:GEL-DMS-Hm21-1KG
/
分子量:5.5
/
Gelest
GEL-DBAZR50-100G
97%
BARIUM ZIRCONIUM (0.33 M)
7到14天内
100g
¥3427
BARIUM ZIRCONIUM (0.33 M)
BARIUM ZIRCONIUM (0.33 M)
货号:GEL-DBAZR50-100G
/
分子式:BaZr(OR)x
/
纯度:97%
/
Gelest
GEL-DMA-131-1KG
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
7到14天内
1kg
¥10575
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
HEXACOSYL TERMINATED POLYDIMETHYLSILOXANE, 65 cSt
货号:GEL-DMA-131-1KG
/
Gelest
GEL-AKT880.5-25G
97%
TITANIUM 1-METHOXY-2-PROPOXIDE
7到14天内
25g
¥2299
TITANIUM 1-METHOXY-2-PROPOXIDE
TITANIUM 1-METHOXY-2-PROPOXIDE
货号:GEL-AKT880.5-25G
/
分子式:C16H36O8Ti
/
分子量:404.35
/
纯度:97%
/
Gelest
GEL-DMGAL50-100G
97%
MAGNESIUM ALUMINUM (1.0M)
7到14天内
100g
¥2717
MAGNESIUM ALUMINUM (1.0M)
MAGNESIUM ALUMINUM (1.0M)
货号:GEL-DMGAL50-100G
/
分子式:MgAl(OR)x
/
纯度:97%
/
Gelest
GEL-PGBLK02-100G
导电性浓缩黑色色素
7到14天内
100g
¥1233
导电性浓缩黑色色素
BLACK PIGMENT CONCENTRATE, CONDUCTIVE
货号:GEL-PGBLK02-100G
/
Gelest
GEL-DBATI50-100G
97%
BARIUM TITANIUM (0.5 M)
7到14天内
100g
¥3051
BARIUM TITANIUM (0.5 M)
BARIUM TITANIUM (0.5 M)
货号:GEL-DBATI50-100G
/
分子式:BaTi(OR)x
/
纯度:97%
/
Gelest
GEL-AKC255-100G
97%
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
7到14天内
100g
¥6855
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
货号:GEL-AKC255-100G
/
分子式:C10H22CuO6
/
分子量:301.83
/
纯度:97%
/
Gelest
GEL-SIO6606.0-25G
97%
十八烷基双(三乙氧基硅基丙基)氯化铵,50%乙醇溶液
7到14天内
25g
¥2487
十八烷基双(三乙氧基硅基丙基)氯化铵,50%乙醇溶液
OCTADECYLBIS(TRIETHOXYSILYLPROPYL)AMMONIUM CHLORIDE, 50% in ethanol
货号:GEL-SIO6606.0-25G
/
分子式:C36H80ClNO6Si2
/
分子量:714.66
/
纯度:97%
/
Gelest
GEL-AKT852.5-10G
97%
TITANIUM DI-s-BUTOXIDE BIS(3,5-HEPTANEDIONATE)
7到14天内
10g
¥6019
TITANIUM DI-s-BUTOXIDE BIS(3,5-HEPTANEDIONATE)
TITANIUM DI-s-BUTOXIDE BIS(3,5-HEPTANEDIONATE)
货号:GEL-AKT852.5-10G
/
分子式:C22H40O6Ti
/
分子量:448.42
/
纯度:97%
/
Gelest
GEL-AKI365-5G
97%
甲氧基乙醇铟,15-18%乙二醇甲醚溶液
7到14天内
5g
¥1504
甲氧基乙醇铟,15-18%乙二醇甲醚溶液
INDIUM METHOXYETHOXIDE, 15-18% in methoxyethanol
货号:GEL-AKI365-5G
/
分子式:C9H21InO6
/
分子量:340.08
/
纯度:97%
/
Gelest
GEL-AKC247-5G
97%
COPPER(II) BENZOYLTRIFLUOROACETONATE
7到14天内
5g
¥4827
COPPER(II) BENZOYLTRIFLUOROACETONATE
COPPER(II) BENZOYLTRIFLUOROACETONATE
货号:GEL-AKC247-5G
/
分子式:C20H12CuF6O4
/
分子量:493.85
/
纯度:97%
/
Gelest
GEL-MTV-112-100G
乙烯基T型聚合物,15-30 cSt
7到14天内
100g
¥3824
乙烯基T型聚合物,15-30 cSt
VINYL T-STRUCTURE POLYMER, 15-30 cSt
货号:GEL-MTV-112-100G
/
Gelest
GEL-DMS-Hm21-100G
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
7到14天内
100g
¥2758
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 100 cSt
货号:GEL-DMS-Hm21-100G
/
分子量:5.5
/
Gelest
GEL-AKI365-25G
97%
甲氧基乙醇铟,15-18%乙二醇甲醚溶液
7到14天内
25g
¥5956
甲氧基乙醇铟,15-18%乙二醇甲醚溶液
INDIUM METHOXYETHOXIDE, 15-18% in methoxyethanol
货号:GEL-AKI365-25G
/
分子式:C9H21InO6
/
分子量:340.08
/
纯度:97%
/
Gelest
GEL-DALZR50-100G
97%
ALUMINUM ZIRCONIUM (0.67 M)
7到14天内
100g
¥1358
ALUMINUM ZIRCONIUM (0.67 M)
ALUMINUM ZIRCONIUM (0.67 M)
货号:GEL-DALZR50-100G
/
分子式:Al2Zr(OR)x
/
纯度:97%
/
Gelest
GEL-AKS725.2-25G
97%
SODIUM ALLYLOXYETHOXIDE, 20% in allyloxyethanol
7到14天内
25g
¥2842
SODIUM ALLYLOXYETHOXIDE, 20% in allyloxyethanol
SODIUM ALLYLOXYETHOXIDE, 20% in allyloxyethanol
货号:GEL-AKS725.2-25G
/
分子式:C5H9NaO2
/
分子量:124.11
/
纯度:97%
/
Gelest
GEL-AKH332-25G
95%
HAFNIUM 2-ETHYLHEXOXIDE, 95%
7到14天内
25g
¥2842
HAFNIUM 2-ETHYLHEXOXIDE, 95%
HAFNIUM 2-ETHYLHEXOXIDE, 95%
货号:GEL-AKH332-25G
/
分子式:C32H68HfO4
/
分子量:695.38
/
纯度:95%
/
Gelest
GEL-AKT878-100G
97%
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
7到14天内
100g
¥4305
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
TITANIUM METHACRYLOXYETHYLACETOACETATE TRIISOPROPOXIDE, 88% in isopropanol
货号:GEL-AKT878-100G
/
分子式:C19H34O8Ti
/
分子量:438.38
/
纯度:97%
/
Gelest
GEL-DMS-LP21-1KG
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
7到14天内
1kg
¥25665
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
货号:GEL-DMS-LP21-1KG
/
分子量:5
/
Gelest
GEL-AKT841-25G
95%
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
7到14天内
25g
¥1672
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
O-ALLYLOXY(POLYETHYLENEOXY)TRIISOPROPOXYTITANATE, 95%
货号:GEL-AKT841-25G
/
分子式:C32H66O14Ti(approx)
/
分子量:660-780
/
纯度:95%
/
Gelest
GEL-AKT816-2.5G
97%
TANTALUM SODIUM METHOXIDE
7到14天内
2.5g
¥2361
TANTALUM SODIUM METHOXIDE
TANTALUM SODIUM METHOXIDE
货号:GEL-AKT816-2.5G
/
分子式:C6H18NaO6Ta
/
分子量:390.14
/
纯度:97%
/
Gelest
GEL-DMGTI50-100G
97%
MAGNESIUM TITANIUM (1.0M)
7到14天内
100g
¥2717
MAGNESIUM TITANIUM (1.0M)
MAGNESIUM TITANIUM (1.0M)
货号:GEL-DMGTI50-100G
/
分子式:MgTi(OR)x
/
纯度:97%
/
Gelest
GEL-PP1-ZPUE-1KG
ZIPCONE(TM) UE
7到14天内
1kg
¥24682
ZIPCONE(TM) UE
ZIPCONE™ UE
货号:GEL-PP1-ZPUE-1KG
/
Gelest
GEL-SIC2266.5-10G
95%
11-(二甲基氯硅基)甲基二十三烷,技术级95%
7到14天内
10g
¥3511
11-(二甲基氯硅基)甲基二十三烷,技术级95%
11-(CHLORODIMETHYLSILYL)METHYLTRICOSANE, tech-95
货号:GEL-SIC2266.5-10G
/
分子式:C26H55ClSi
/
分子量:431.27
/
纯度:95%
/
Gelest
GEL-DMGAL30-25G
97%
MAGNESIUM ALUMINUM (0.75M)
7到14天内
25g
¥836
MAGNESIUM ALUMINUM (0.75M)
MAGNESIUM ALUMINUM (0.75M)
货号:GEL-DMGAL30-25G
/
分子式:MgAl2(OR)x
/
纯度:97%
/
Gelest
GEL-DMS-CA21-100G
双(羟乙基)氨基封端的聚二甲基硅氧烷,120-160 cSt
7到14天内
100g
¥3699
双(羟乙基)氨基封端的聚二甲基硅氧烷,120-160 cSt
[BIS(HYDROXYETHYL)AMINE] TERMINATED POLYDIMETHYLSILOXANE, 120-160 cSt
货号:GEL-DMS-CA21-100G
/
分子量:3000
/
Gelest
GEL-HDP-111-25G
氢基封端的聚苯基-(二甲基氢基硅烷)硅氧烷,50-80 cSt
7到14天内
25g
¥877
氢基封端的聚苯基-(二甲基氢基硅烷)硅氧烷,50-80 cSt
POLYPHENYL-(DIMETHYLHYDROSILOXY)SILOXANE, HYDRIDE TERMINATED, 50-80 cSt
货号:GEL-HDP-111-25G
/
Gelest
GEL-DMS-CS26-100G
100%
(2-羟基-3-甲氧基丙氧基)丙基封端聚二甲基硅氧烷
7到14天内
100g
¥11745
(2-羟基-3-甲氧基丙氧基)丙基封端聚二甲基硅氧烷
(2-HYDROXY-3-METHOXYPROPOXY)PROPYL TERMINATED POLYDIMETHYLSILOXANE
货号:GEL-DMS-CS26-100G
/
纯度:100%
/
Gelest
GEL-AKT843-25G
97%
TITANIUM ALLYLACETOACETATETRAIISOPROPOXIDE
7到14天内
25g
¥2194
TITANIUM ALLYLACETOACETATETRAIISOPROPOXIDE
TITANIUM ALLYLACETOACETATETRIISOPROPOXIDE
货号:GEL-AKT843-25G
/
分子式:C16H30O6Ti
/
分子量:358.25
/
纯度:97%
/
Gelest
GEL-DGM-000-1KG
DIMETHYLSILOXANE GUM
7到14天内
1kg
¥5057
DIMETHYLSILOXANE GUM
DIMETHYLSILOXANE GUM
货号:GEL-DGM-000-1KG
/
Gelest
GEL-VMS-005-100G
乙烯基甲基硅氧烷均聚物,环状,3-7 cSt
7到14天内
100g
¥1588
乙烯基甲基硅氧烷均聚物,环状,3-7 cSt
VINYLMETHYLSILOXANE HOMOPOLYMER, cyclics, 3-7 cSt
货号:GEL-VMS-005-100G
/
分子量:258-431
/
Gelest
GEL-DMS-S33M50-3KG
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
7到14天内
3kg
¥3323
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
货号:GEL-DMS-S33M50-3KG
/
Gelest
GEL-AKC242-1G
97%
COPPER(II) ALLYLOXYETHOXYTRIFLUOROACETOACETATE
7到14天内
1g
¥5183
COPPER(II) ALLYLOXYETHOXYTRIFLUOROACETOACETATE
COPPER(II) ALLYLOXYETHOXYTRIFLUOROACETOACETATE
货号:GEL-AKC242-1G
/
分子式:C18H20CuF6O8
/
分子量:541.89
/
纯度:97%
/
Gelest
GEL-CXTI038-25G
TITANIUM 3,6-DIOXAHEPTANOATE
7到14天内
25g
¥3950
TITANIUM 3,6-DIOXAHEPTANOATE
Titanium 3,6-Dioxaheptanoate, Tech-95
货号:GEL-CXTI038-25G
/
分子式:C20H36O16Ti
/
分子量:530.38
/
Gelest
GEL-DINSN20-25G
97%
INDIUM TIN
7到14天内
25g
¥3302
INDIUM TIN
INDIUM TIN
货号:GEL-DINSN20-25G
/
分子式:InSn3(OR)x
/
纯度:97%
/
Gelest
GEL-DMS-S33M50-18KG
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
7到14天内
18kg
¥7147
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
货号:GEL-DMS-S33M50-18KG
/
Gelest
GEL-DBP-V052-100G
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
7到14天内
100g
¥2612
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
货号:GEL-DBP-V052-100G
/
分子量:8,000-10,000
/
Gelest
GEL-AKC255-25G
97%
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
7到14天内
25g
¥2131
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
COPPER(II) METHOXYETHOXYETHOXIDE, 10-12% in methoxyethoxyethanol
货号:GEL-AKC255-25G
/
分子式:C10H22CuO6
/
分子量:301.83
/
纯度:97%
/
Gelest
GEL-DMS-Hm15-1KG
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
7到14天内
1kg
¥20544
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
货号:GEL-DMS-Hm15-1KG
/
分子量:3,000-3,500
/
Gelest
GEL-DALY080-100G
97%
ALUMINUM YTTRIUM
7到14天内
100g
¥5204
ALUMINUM YTTRIUM
ALUMINUM YTTRIUM
货号:GEL-DALY080-100G
/
分子式:Al3Y(OR)x
/
纯度:97%
/
Gelest
GEL-DCS-8024-1KG
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
7到14天内
1kg
¥16155
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
(78-82% POLYDIMETHYLSILOXANE)-SILETHYLPHENYLENE COPOLYMER, 350-600 cSt
货号:GEL-DCS-8024-1KG
/
分子量:5,000-6,000
/
Gelest
GEL-DALZR50-500G
97%
ALUMINUM ZIRCONIUM (0.67 M)
7到14天内
500g
¥5392
ALUMINUM ZIRCONIUM (0.67 M)
ALUMINUM ZIRCONIUM (0.67 M)
货号:GEL-DALZR50-500G
/
分子式:Al2Zr(OR)x
/
纯度:97%
/
Gelest
GEL-DMS-S33M50-100G
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
7到14天内
100g
¥438
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
SILANOL TERMINATED POLYDIMETHYLSILOXANE, EMULSION
货号:GEL-DMS-S33M50-100G
/
Gelest
GEL-PMS-H03-100G
氢基封端的聚苯基甲基硅氧烷,2-5 cSt
7到14天内
100g
¥4138
氢基封端的聚苯基甲基硅氧烷,2-5 cSt
POLYPHENYLMETHYLSILOXANE, HYDRIDE TERMINATED, 2-5 cSt
货号:GEL-PMS-H03-100G
/
分子量:300-500
/
Gelest
GEL-AKH334-25G
95%
HAFNIUM n-OCTOXIDE, 95%
7到14天内
25g
¥2487
HAFNIUM n-OCTOXIDE, 95%
Hafnium n-Octoxide, 95%
货号:GEL-AKH334-25G
/
分子式:C32H68HfO4
/
分子量:695.38
/
纯度:95%
/
Gelest
GEL-DMS-T72B15-100G
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
7到14天内
100g
¥1483
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
货号:GEL-DMS-T72B15-100G
/
Gelest
GEL-DINSN20-100G
97%
INDIUM TIN
7到14天内
100g
¥10700
INDIUM TIN
INDIUM TIN
货号:GEL-DINSN20-100G
/
分子式:InSn3(OR)x
/
纯度:97%
/
Gelest
GEL-HDP-111-100G
氢基封端的聚苯基-(二甲基氢基硅烷)硅氧烷,50-80 cSt
7到14天内
100g
¥2633
氢基封端的聚苯基-(二甲基氢基硅烷)硅氧烷,50-80 cSt
POLYPHENYL-(DIMETHYLHYDROSILOXY)SILOXANE, HYDRIDE TERMINATED, 50-80 cSt
货号:GEL-HDP-111-100G
/
Gelest
GEL-DMS-LP21-100G
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
7到14天内
100g
¥3824
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
CHLOROMETHYLPHENETHYL TERMINATED POLYDIMETHYLSILOXANE, 100-150 cSt
货号:GEL-DMS-LP21-100G
/
分子量:5000
/
Gelest
GEL-DMS-T72B15-3KG
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
7到14天内
3kg
¥8151
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
POLYDIMETHYLSILOXANE, TRIMETHYLSILOXY TERMINATED, BLEND, 4,000-8,000 cSt
货号:GEL-DMS-T72B15-3KG
/
Gelest
GEL-ATM-1322M50-3KG
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
7到14天内
3kg
¥2884
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
货号:GEL-ATM-1322M50-3KG
/
Gelest
GEL-DMS-Hm15-100G
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
7到14天内
100g
¥2967
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
MONODISPERSE HYDRIDE TERMINATED POLYDIMETHYLSILOXANE, 50 cSt
货号:GEL-DMS-Hm15-100G
/
分子量:3,000-3,500
/
Gelest
GEL-DMGZR50-25G
97%
MAGNESIUM ZIRCONIUM (1.0M)
7到14天内
25g
¥1086
MAGNESIUM ZIRCONIUM (1.0M)
MAGNESIUM ZIRCONIUM (1.0M)
货号:GEL-DMGZR50-25G
/
分子式:MgZr(OR)x
/
纯度:97%
/
Gelest
GEL-MCR-B12-100G
不对称的单羧基癸基封端基聚二甲基硅氧烷,20 cSt
7到14天内
100g
¥6228
不对称的单羧基癸基封端基聚二甲基硅氧烷,20 cSt
MONOCARBOXYDECYL TERMINATED POLYDIMETHYLSILOXANE, asymmetric, 20 cSt
货号:GEL-MCR-B12-100G
/
分子量:1500
/
Gelest
GEL-DBP-V052-1KG
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
7到14天内
1kg
¥15549
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
DIMETHYLSILOXANE-VINYLMETHYLSILOXANE - (PROPYLENE OXIDE-ETHYLENE OXIDE) BLOCK COPOLYMER, 500-600 cSt
货号:GEL-DBP-V052-1KG
/
分子量:8,000-10,000
/
Gelest
GEL-DMGZR50-100G
97%
MAGNESIUM ZIRCONIUM (1.0M)
7到14天内
100g
¥3511
MAGNESIUM ZIRCONIUM (1.0M)
MAGNESIUM ZIRCONIUM (1.0M)
货号:GEL-DMGZR50-100G
/
分子式:MgZr(OR)x
/
纯度:97%
/
Gelest
GEL-AKS734-25G
SODIUM DIISOPROPYLDITHIOCARBAMATE, tech-90
7到14天内
25g
¥3051
SODIUM DIISOPROPYLDITHIOCARBAMATE, tech-90
Sodium Diisopropyldithiocarbamate, Tech-90
货号:GEL-AKS734-25G
/
分子式:C7H14NNaS2
/
分子量:199.31
/
Gelest
GEL-SIA0599.4-25G
65%
N-3-[(AMINO(POLYPROPYLENOXY)]AMINOPROPYLTRIMETHOXYSILANE, 60 - 65%
7到14天内
25g
¥2988
N-3-[(AMINO(POLYPROPYLENOXY)]AMINOPROPYLTRIMETHOXYSILANE, 60 - 65%
N-3-[(AMINO(POLYPROPYLENOXY)]AMINOPROPYLTRIMETHOXYSILANE, 60 - 65%
货号:GEL-SIA0599.4-25G
/
分子量:337-435
/
纯度:65%
/
Gelest
GEL-PP2-OE41.2-1KG
GELEST OE(TM) 41.2 Accelerated Cure
7到14天内
1kg
¥3323
GELEST OE(TM) 41.2 Accelerated Cure
GELEST OE™ 41.2 Accelerated Cure
货号:GEL-PP2-OE41.2-1KG
/
Gelest
GEL-PP1-GC18-100G
Glassclad 18
7到14天内
100g
¥710
Glassclad 18
Glassclad® 18
货号:GEL-PP1-GC18-100G
/
Gelest
GEL-ATM-1322M50-18KG
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
7到14天内
18kg
¥7147
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
AMINOETHYLAMINOPROPYLMETHOXYSILOXANE - DIMETHYLSILOXANE COPOLYMER, BRANCHED, EMULSION
货号:GEL-ATM-1322M50-18KG
/
Gelest
GEL-DLITA050-10G
97%
LITHIUM TANTALUM
7到14天内
10g
¥2988
LITHIUM TANTALUM
LITHIUM TANTALUM
货号:GEL-DLITA050-10G
/
分子式:LiTa(OR)x
/
纯度:97%
/
Gelest
GEL-DMGAL30-100G
97%
MAGNESIUM ALUMINUM (0.75M)
7到14天内
100g
¥2717
MAGNESIUM ALUMINUM (0.75M)
MAGNESIUM ALUMINUM (0.75M)
货号:GEL-DMGAL30-100G
/
分子式:MgAl2(OR)x
/
纯度:97%
/
Gelest
GEL-VMS-005-3KG
乙烯基甲基硅氧烷均聚物,环状,3-7 cSt
7到14天内
3kg
¥7022
乙烯基甲基硅氧烷均聚物,环状,3-7 cSt
VINYLMETHYLSILOXANE HOMOPOLYMER, cyclics, 3-7 cSt
货号:GEL-VMS-005-3KG
/
分子量:258-431
/
Gelest
GEL-AKT880.5-100G
97%
TITANIUM 1-METHOXY-2-PROPOXIDE
7到14天内
100g
¥7315
TITANIUM 1-METHOXY-2-PROPOXIDE
TITANIUM 1-METHOXY-2-PROPOXIDE
货号:GEL-AKT880.5-100G
/
分子式:C16H36O8Ti
/
分子量:404.35
/
纯度:97%
/
Gelest
GEL-DALY080-25G
97%
ALUMINUM YTTRIUM
7到14天内
25g
¥1609
ALUMINUM YTTRIUM
ALUMINUM YTTRIUM
货号:GEL-DALY080-25G
/
分子式:Al3Y(OR)x
/
纯度:97%
/