货号 | 包装规格 | 库存状态 | 价格 | 说明 | 数量 | ||
---|---|---|---|---|---|---|---|
S433662-25g | 25g | 现货 | ¥4727.92 | ||||
S433662-5g | 5g | 现货 | ¥1312.72 |
规格或纯度:MCM-41型(六角)
英文名称:Silica, mesostructured
别名:二氧化硅
英文别名:Silica, Silicon dioxide
产品介绍:一般描述 介孔结构二氧化硅(MCM-41)是低密度有序介孔硅酸盐体系的一部分,该体系具有2D六方相,其是在季铵卤化表面活性剂存在下进行制备。它的孔有序且大,直径在1.5-10 nm之间,比表面积为1500 m 2 /g。 应用 MCM-41可作为基底材料,与铂配合物组装形成发光氧传感材料。它也可以用作捕获CO 2 的吸附剂。表面官能化的MCM-41可用作双酚A合成中的催化剂。 General Description Silica, mesostructured (MCM-41) is a part of low-density organized mesoporous silicate system which has a 2D hexagonal phase, prepared in the presence of quaternary ammonium halide surfactant. It has ordered and large pores with diameter in the range 1.5-10 nm and specific surface area of 1500 m 2 /g. Application MCM-41 may be used as a base material that can be assembled with platinum complexes to develop luminescent oxygen sensing materials. It may also be used as an adsorbent in CO 2 capture application. Surface functionalized MCM-41 may be used as a catalyst in the synthesis of bisphenol A.
EC号:238-878-4
IUPAC Name:dioxosilane
INCHI:InChI=1S/O2Si/c1-3-2
InChi Key:VYPSYNLAJGMNEJ-UHFFFAOYSA-N
Canonical SMILES:O=[Si]=O
分子式:
SiO2
关联CAS:60676-86-0
PubChem CID:24261
分子量:60.08
沸点:2230°C
熔点:1670°C
象形图:
信号词:Danger
危险声明:H351: Suspected of causing cancer H373: Causes damage to organs through prolonged or repeated exposure H332: Harmful if inhaled H372: Causes damage to organs through prolonged or repeated exposure H371: May cause damage to organs
预防措施声明:P261,P280,P405,P501,P264,P260,P271,P270,P304+P340,P203,P318,P317,P308+P316,P319
RTECS:VV7330000
个人防护装备:dust mask type N95 (US), Eyeshields, Gloves